Answer Key: Self-Test B-6.4

  1. a. 1″
  2. a. 20–30° off perpendicular in direction of travel
  3. a. Electrode too far from work
  4. a. Rate of travel that is too fast
  5. c. Porosity
  6. c. Lack of fusion
  7. a. Incorrect joint design
  8. b. High-alloy steel
  9. c. Welding has been interrupted
  10. d. Cleaning all slag from the surface of the previous bead
  11. c. Improper electrode manipulation
  12. d. Uneven expansion and contraction within a metal
  13. a. Pre-bending
  14. d. Single vee butt joint
  15. a. Overlap